Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.05 MPa @Thickness 3.20 mm |
3633 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HYPERIER IP1306B PA-HDPE Nanoclay Compound HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPEApplication: Agrochemical Container, SORE* Fuel Tank, PFCCAS No. 900.. |
|||
Tensile Strength, Yield | 25.05 MPa | 3633 psi | ASTM D412 |
Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D198K is an aliphatic based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss aspect†on the f.. |