Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.39 MPa | 3683 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 25.39 MPa | 3683 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 25.39 MPa | 3683 psi | |
C.O.I.M. PLAXTER® P 52 Polymeric Plasticizer Description: Formulated with PVC, it is used for the production of insulated cables and stretching films.Information provided by P.A.T. Products, Inc. |