Polymer Property : Tensile Strength, Yield = 253 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 253 MPa
36700 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength, Yield 253 MPa
36700 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength, Yield 253 MPa
36700 psi
ASTM D 638
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66
LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
Tensile Strength, Yield 253 MPa
36700 psi
ISO 527
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66
LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
Tensile Strength, Yield 253 MPa
36700 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength, Yield 253 MPa
36700 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength, Yield 253 MPa
36700 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66
LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength, Yield 253 MPa
36700 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66
LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized.