Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.7 MPa
3870 psi
64% Ret.
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 26.7 MPa
3870 psi
ASTM D638
Entec Hypro™ PPC-T30 Copolymer Polypropylene, 30% Talc Reinforced
Information provided by Entec