Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G67P Translucent Perfluoroelastomer A translucent beige compound with semi-crystalline perfluoropolymer nano-filler, specially developed to meet the demands of the semiconductor and bio-analytical industries. Compatible with fluorine .. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D412 |
Precision Polymer Engineering Z85L Hydrogenated NBR Compound Peroxide Cured, Hydrogenated Nitrile Rubber, 81-90 °IRHD. Low acrylonitrile content.Applications: Specially compounded for service in low-temperature applications. High strength and excellent chem.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D-638 |
Axiall 17890 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for THW and 90C Class 43 applications. UL recognized component for THW and TW.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D-638 |
Axiall 18901 Wire & Cable Flexible PVC General purpose, non-lead stabilized, 105°C rated jacketing compound. Formulated to have good migration resistance and flame retardant properties.Information provided by Georgia GulfGeorgia Gulf b.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D-638 |
Axiall 34551 Wire & Cable Flexible PVC TW, THW insulation also suitable for 105°C AWM, flex cords and Class 12/12B insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D-638 |
Axiall 16901 Wire & Cable Flexible PVC 90°C rated fiber optic riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D638 |
Resirene Resirene® 8450 High Impact Polystyrene (Chemical Resistant) Features:Low FlowChemical ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingRegistration LinersExtruded SheetInformation provided by US distributor Calsak Co.. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D-638 |
Axiall 38901 Wire & Cable Flexible PVC Non-lead flame retardant flexible PVC compound suitable for integral conduit jackets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 18.3 MPa | 2650 psi | ASTM D-638 |
Axiall 54915 Moldings & Extrusions Flexible PVC Medium durometer injection molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |