Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.4 MPa | 3970 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® SM840 Polypropylene impact copolymer Titanpro® SM840 is an extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvant.. |
|||
Tensile Strength, Yield | 27.4 MPa | 3980 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® H5234 High Density Polyethylene ApplicationsALATHON H 5234 is a high flow injection molding grade of resin designed for fast cycle and thin wall molding. It provides cold temperature impact resistance. Typical applications inclu.. |