Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.189 MPa | 27.4 psi | ASTM D3574 |
Lendell Nolatex® Latex Free Foam This foam is used in the cosmetics industry and also possesses insulation qualities.Applications:Cosmetic Wedges and Puffs, Padding, High Insulative Value Applications, Makovers ® Disposable Make.. |