Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 187 MPa | 27100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Tensile Strength, Yield | 187 MPa | 27100 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 CF30 TL12 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance and Lo.. |