Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.8 MPa | 2720 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |