Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.14 MPa | 2776 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 115-1008 LMDPE Rotational Molding Resin Description: ICORENE 115-1008 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Tensile Strength, Yield | 19.14 MPa | 2776 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 115-1650 LMDPE Rotational Molding Resin Description: ICORENE 115-1650 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Tensile Strength, Yield | 19.14 MPa | 2776 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 115-1653 LMDPE Rotational Molding Resin Description: ICORENE 115-1653 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |