Polymer Property : Tensile Strength, Yield = 28.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.10 MPa
4075 psi
after 7 days at 100ºC
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.5 PHR Sulfur
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 28.10 MPa
4075 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 28.10 MPa
4075 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 28.10 MPa
4075 psi
after 7 days at 100ºC
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.5 PHR Sulfur
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 28.10 MPa
4075 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 28.10 MPa
4075 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..