Polymer Property : Tensile Strength, Yield = 28.99 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.99 MPa
4205 psi
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..
Tensile Strength, Yield 28.99 MPa
4205 psi
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..