Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 2800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.4 - 19.3 MPa
1800 - 2800 psi
Average value: 18.0 MPa Grade Count:71
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Tensile Strength, Yield 11.7 - 19.3 MPa
1700 - 2800 psi
ASTM D638
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Copyright © lookpolymers.com All Rights Reserved