Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 194 MPa | 28200 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Tensile Strength, Yield | 194 MPa | 28200 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF40 HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Tensile Strength, Yield | 194 MPa | 28200 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF40 UV L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceAppearan.. |
|||
Tensile Strength, Yield | 194 MPa | 28200 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF40 FR HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |