Tensile Strength, Yield 0.866 - 195 MPa
126 - 28300 psi
Average value: 138 MPa Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Tensile Strength, Yield 60.0 - 195 MPa
8700 - 28300 psi
Average value: 114 MPa Grade Count:91
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..