Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.00 MPa
2901 psi
At 50 mm/min; ISO/DIS 6259
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))
BorPEX ME2510 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for crosslinkab..