Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.1 MPa | 2910 psi | ASTM D412 |
Polymax® Maxelast® A9875H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 20.1 MPa | 2910 psi | ASTM D412 |
Teknor Apex APEX® 90-P513A-85-NT Polyvinyl Chloride+PUR Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | >= 20.1 MPa | >= 2910 psi | ASTM D638 |
Buckeye Polymers BP RPP 1012 T BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |