Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.56 MPa
516 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5407 Nitrile Rubber
General purpose Nitrile; Peroxide curedInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 3.56 MPa
516 psi
ASTM D412
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer
Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer ..