Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.575 MPa | 518.5 psi | -35% change after 336 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering F70R Fluorosilicone Rubber Red Fluorosilicone, 65-75 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 70.Applications: S.. |