Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.92 MPa | 569 psi | ASTM D412 |
Polymax® Maxelast® A9840 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 3.92 MPa | 569 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Tensile Strength, Yield | 3.92 MPa | 569 psi | at 100% elongation, maximum |
Dow Corning SILASTIC® 37087-V SILICONE RUBBER NATURAL 70 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning |
|||
Tensile Strength, Yield | 3.92 MPa | 569 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-550 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.92 MPa | 569 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-550 Dow-Corning Class VI Elastomer Information provided by Multibase |