Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding 50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced Nylon 6, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-30CF/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 %, Temperature 760 °C |
30000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 207 - 345 MPa @Strain 0.200 % |
30000 - 50000 psi @Strain 0.200 % |
Annealed temper |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 IM 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingIn.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF60 X 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-01027 A 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ISO 527 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ISO 527 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton RV008ESV PA 66 40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 207 - 303 MPa | 30000 - 44000 psi | 0.2% offset |
Eagle Brass 110 EPT COPPER, 1/2 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Yield | >= 207 MPa | >= 30000 psi | 0.2% Offset |
Eagle Brass 316 Austenitic Stainless Steel, Annealed The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Tensile Strength, Yield | >= 207 MPa | >= 30000 psi | 0.2% Offset |
Eagle Brass 430 Ferritic Stainless Steel, Annealed Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 % |
30000 psi @Strain 0.200 % |
|
Crucible Steel 316L Chromium-Nickel Steel Crucible 316L is a non-hardenable, low carbon austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Crucible 316L is designed for special applications requiring resi.. |
|||
Tensile Strength, Yield | 207 - 303 MPa | 30000 - 44000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), 1/2 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | 207 - 303 MPa | 30000 - 44000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Yield | >= 207 MPa | >= 30000 psi | 0.2% Offset |
Eagle Brass 304 Austenitic Stainless Steel, Annealed Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 207 MPa @Strain 0.200 % |
>= 30000 psi @Strain 0.200 % |
|
Carlson 317L 4 Austenitic Stainless Steel General DescriptionCarlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel a.. |
|||
Tensile Strength, Yield | >= 207 MPa @Strain 0.200 % |
>= 30000 psi @Strain 0.200 % |
|
Carlson 317L Austenitic Stainless Steel Carlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel and molybdenum prese.. |
|||
Tensile Strength, Yield | >= 207 MPa @Strain 0.200 % |
>= 30000 psi @Strain 0.200 % |
|
Carlson C 800 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists.. |
|||
Tensile Strength, Yield | 207 MPa @Strain 0.200 %, Temperature 427 °C |
30000 psi @Strain 0.200 %, Temperature 801 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | >= 207 MPa | >= 30000 psi | Annealed |
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 207 MPa @Temperature 427 °C |
30000 psi @Temperature 801 °F |
Annealed |
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du.. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific) LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. |
|||
Tensile Strength, Yield | 207 MPa | 30000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF50 FR-N BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |