Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 206.9 MPa
>= 30010 psi
ATI Allegheny Ludlum Type 310L Stainless Steel
Corrosive attack of stainless steels by concentrated nitric acid often results in preferential attack of grain boundaries. The high Cr content combined with restricted levels of C, Si, P, S, and Mo ..