Mechanical Properties Metric English Comments
Tensile Strength, Yield 314 MPa
45500 psi
Kennametal Stellite Stellite® 250
Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace..
Tensile Strength, Yield 314 MPa

@Strain 0.200 %
45500 psi

@Strain 0.200 %
Haynes HR-160® alloy, hot rolled and solution annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Yield 314 MPa

@Strain 0.200 %
45500 psi

@Strain 0.200 %
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..