Polymer Property : Tensile Strength, Yield = 325 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 325 MPa

@Strain 0.200 %
47100 psi

@Strain 0.200 %
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Tensile Strength, Yield 325 MPa

@Strain 0.200 %,
Temperature 870 °C
47100 psi

@Strain 0.200 %,
Temperature 1600 °F
Haynes 25 alloy, cold worked sheet, 10% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 325 MPa

@Strain 0.200 %,
Temperature 205 °C
47100 psi

@Strain 0.200 %,
Temperature 401 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Tensile Strength, Yield 325 - 385 MPa
47100 - 55800 psi
ArcelorMittal HSLA 320 High strength low alloy steel for cold forming, Hot Rolled
Available in the following: S315MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w..
Tensile Strength, Yield 325 MPa

@Strain 0.200 %
47100 psi

@Strain 0.200 %
Haynes 230® alloy, as cast vacuum investment casting
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..