Tensile Strength, Yield 33.22 MPa
4819 psi
3.5% change after 70 hours @ 150°C; ASTM D412
Precision Polymer Engineering Z95X Hydrogenated NBR Compound
Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applica..