Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.6 MPa
4870 psi
ASTM D638
Styron Magnumâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS)
High Impact, High Heat, Blow Molding ABSInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Yield 33.6 MPa
4870 psi
ASTM D638
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron
Tensile Strength, Yield 33.6 MPa
4870 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 290ºF Cure Temperature
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tensile Strength, Yield 33.6 MPa
4870 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 290ºF Cure Temperature
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..