Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 34.1 MPa | 4950 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 30-0300 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 34.1 MPa | 4950 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.1 MPa | 4950 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.1 MPa | 4940 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 34.1 MPa | 4940 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |