Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.7 MPa | 3440 psi | ASTM D638 Type IV |
Chevron Phillips Marlex® C513 High density polyethylene
(discontinued **) Benefits: outstanding impact and creep resistance, outstanding ESCR, excellent processabilityApplications: intermediate bulk containers, agricultural containersInformation provided by Chevron Philli.. |
|||
Tensile Strength, Yield | 23.7 MPa | 3440 psi | Crosshead speed 100 mm/min; ISO 527 |
SCG Chemicals EL-Leneâ„¢ H5211PBR High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Non pressure pipes, co-extruded pipes as the inner layerInformation provided by SCG Chemicals |