Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.28 MPa | 3522 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Benzoflex 9-88SG Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 24.28 MPa | 3522 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Benzoflex 9-88SG Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |