Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.9 MPa | 3760 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP 600 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP H6 GF25 NHFR grey Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | ASTM D638 |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CM005 Polypropylene Impact Copolymer COPYLENE® CM005 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes..Applications: Extrusion, sheet, film.Infor.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2 in/min; ASTM D638 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | ASTM D638 |
Dow C700-35 Polypropylene Impact Copolymer Resin OverviewHigh stiffnessGood mold fillabilityComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C700-35 Polypropylene Resin is intended for use in injection molding processes where medium .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | ASTM D638 |
Entec Hypro™ PPC-T40 Copolymer Polypropylene, 40% Talc Reinforced Information provided by Entec |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | |
C.O.I.M. PLAXTER® P 42 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |