Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.5 MPa
5580 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Strength, Yield 38.5 MPa
5580 psi
Ineos ABS Centrex® 814 ASA Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba..
Tensile Strength, Yield 38.5 MPa
5580 psi
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Tensile Strength, Yield 38.5 MPa
5580 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers Centrex® 814 General Purpose Injection Molding Grade
Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing perfor..