Polymer Property : Tensile Strength, Yield = 383 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 383 MPa

@Strain 0.200 %
55500 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 383 MPa

@Strain 0.200 %
55500 psi

@Strain 0.200 %
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, Solution Treated
Tensile strength (ultimate and yield), and elongation values reported here are typical for Cold Rolled Sheet, Solution Treated samples. Density and magnetic permeability are typical of annealed INCO..