Tensile Strength, Yield 385 MPa

@Strain 0.200 %
55800 psi

@Strain 0.200 %
Haynes 230® alloy, 10% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 385 MPa

@Strain 0.200 %
55800 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 385 MPa

@Strain 0.200 %
55800 psi

@Strain 0.200 %
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
Tensile Strength, Yield 385 MPa

@Strain 0.200 %
55800 psi

@Strain 0.200 %
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..