Polymer Property : Tensile Strength, Yield = 3860 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.6 MPa
3860 psi
50 mm/min; ASTM D638
ICO Polymers ICORENEâ„¢ 150-1501 HDPE Rotational Molding Resin
Description: ICORENE 150-1501 is a high density polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability..
Tensile Strength, Yield 26.6 MPa
3860 psi
ASTM D1458
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Tensile Strength, Yield 26.6 MPa
3860 psi
Spartech E66091 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Tensile Strength, Yield 26.6 MPa
3860 psi
2.0 in/min; ASTM D638
ExxonMobil AP03B Polypropylene Impact Copolymer
Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio..
Tensile Strength, Yield 26.6 MPa
3860 psi
Type 1 @ 2.0 in/min; ASTM D-638
Chevron Phillips K-Resin® KR03BR SBC  (discontinued **)
K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:BottlesMolded boxes and containersMedical devicesPortion packagesBlister packagingFeatures:Good stiffnessGood formabilityGood toughnessExcelle..