Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.69 MPa
390 psi
at 200%, as molded
Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 2.69 MPa
390 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-150 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 2.69 MPa
390 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 2.69 MPa
390 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 2.69 MPa
390 psi
at 200%, molded-without post cure; ASTM D412
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 2.69 MPa
390 psi
100%; ASTM D412
Teknor Apex APEX® 3210-55 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 2.69 MPa
390 psi
100%; ASTM D412
Teknor Apex APEX® 3211-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 2.69 MPa
390 psi
100%; ASTM D412
Teknor Apex Flexalloy® 3501-45-NT Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe..