Polymer Property : Tensile Strength, Yield = 392.3 MPa
Polymer Property :
Tensile Strength, Yield =
392.3 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
>=
392.3
MPa
>=
56900
psi
Crucible Steel 21-12N (JIS SUH37) Martensitic Steel
Information provided by Crucible Specialty Metals.