Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.24 MPa
615 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Strength, Yield 4.24 MPa

@Strain 300 %
615 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3870E Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A ther..
Tensile Strength, Yield 4.24 MPa

@Strain 300 %
615 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 62-001 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Over-Molding GradeNaturalTransparentUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.