Tensile Strength, Yield 4.42 MPa
641 psi
ASTM D412
Polymax® Maxelast® P1860D TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 4.42 MPa
641 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5514 Polyacrylate Rubber
General purpose Natural RubberInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 4.42 MPa
641 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7157 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.