Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.51 MPa | 654 psi | ASTM D412 |
Polymax® Maxelast® P2755 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.51 MPa | 654 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |