Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.71 MPa
683 psi
ASTM D412
Polymax® Maxelast® P3755 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 4.71 MPa
683 psi
at 300% elongation; ASTM D412
Lubrizol Estane® T365A Thermoplastic Polyurethane
Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..