Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.1 MPa
5810 psi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b..
Tensile Strength, Yield 40.1 MPa
5810 psi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded..