Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2760 MPa | 400000 psi | Typical epoxy composite property |
Hexcel® HexTow™ IM6 Carbon Fiber HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized .. |
|||
Tensile Strength, Yield | 2760 MPa | 400000 psi | Typical epoxy composite property |