Mechanical Properties Metric English Comments
Tensile Strength, Yield 283 MPa

@Strain 0.200 %
41000 psi

@Strain 0.200 %
FloMet 7% Ni/Fe Low Alloy Steel
FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume..
Tensile Strength, Yield 283 MPa

@Strain 0.200 %,
Temperature 427 °C
41000 psi

@Strain 0.200 %,
Temperature 801 °F
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 283 MPa

@Strain 0.200 %,
Temperature 427 °C
41000 psi

@Strain 0.200 %,
Temperature 801 °F
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield >= 283 MPa
>= 41000 psi
Alcoa UltrAlloy® 6020-T8 Aluminum
Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi..
Tensile Strength, Yield 283 - 345 MPa
41000 - 50000 psi
0.2% offset
Eagle Brass 110 EPT COPPER, Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Tensile Strength, Yield 283 - 345 MPa
41000 - 50000 psi
0.2% offset
Eagle Brass 101 OFE COPPER (Certified), Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Tensile Strength, Yield 283 - 345 MPa
41000 - 50000 psi
0.2% offset
Eagle Brass 102 OF COPPER (Non-Certified), Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Tensile Strength, Yield >= 283 MPa

@Strain 0.200 %
>= 41000 psi

@Strain 0.200 %
Carlson GOC 276 Nickel-Molybdenum-Chromium
General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in ..
Tensile Strength, Yield 283 MPa

@Strain 0.200 %
41000 psi

@Strain 0.200 %
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Tensile Strength, Yield >= 283 MPa

@Strain 0.200 %
>= 41000 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276
AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount..
Tensile Strength, Yield 283 MPa

@Strain 0.200 %,
Temperature 760 °C
41000 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Tensile Strength, Yield 283 MPa

@Strain 0.200 %,
Temperature 204 °C
41000 psi

@Strain 0.200 %,
Temperature 399 °F
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated