Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 159 - 283 MPa | 23000 - 41000 psi | 0.2% offset |
Eagle Brass 770 Nickel Silver 18%, Annealed 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Yield | 241 - 283 MPa @Strain 0.200 %, Thickness 1.02 - 1.78 mm |
35000 - 41000 psi @Strain 0.200 %, Thickness 0.0400 - 0.0700 in |
Annealed Condition |
AK Steel 409 Ferritic Stainless steel AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applicatio.. |