Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 288 MPa @Temperature 190 °C |
41800 psi @Temperature 374 °F |
Laminate property; Open Hole Tension; Conditioning: 158°F 85% RH sat |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |