Tensile Strength, Yield 294 MPa

@Strain 0.200 %
42600 psi

@Strain 0.200 %
Typical; after 1800°F Anneal
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800
Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both ..