Polymer Property : Tensile Strength, Yield = 42800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Temperature 540 °C
42800 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Temperature 650 °C
42800 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %
42800 psi

@Strain 0.200 %
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %
42800 psi

@Strain 0.200 %
Typical; Annealed at 1800°F (982°C)
ATI Allegheny Ludlum AL 800™ Nickel-Base Alloy, UNS N08800
AL 800 alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-corr..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Temperature 760 °C
42800 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %
42800 psi

@Strain 0.200 %
Haynes 556® alloy, bar, after 4000 hours at 870°C (1600°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..