Polymer Property : Tensile Strength, Yield = 429 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 429 MPa

@Strain 0.200 %
62200 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged at 649°C (1200°F) for 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 429 MPa

@Strain 0.200 %
62200 psi

@Strain 0.200 %
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..