Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 30.10 MPa | 4365 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 30.10 MPa | 4365 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 30.10 MPa | 4365 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 30.10 MPa | 4365 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 30.10 MPa | 4365 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 30.10 MPa | 4365 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |