Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47 ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47N ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | |
Ineos ABS Lustran® 2863
(discontinued **) Special grade for smart cards.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RE 625 Rigid PVC, Extrusion Spiral pipes |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RK 218 Rigid PVC, Extrusion Lead Free Rolling shutters |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 200°C for 1,000 hrs; ASTM D1458 |
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific) Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | |
Styrolution NOVODUR® P2H-AT ABS, Injection Grade Standard injection molding grade, easy flow, high gloss, hard, antistatic.Applications: Telephones, household goods, video and audio industry, office equipment. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EZ250 PPE+PS Automotive wheel covers. Offers superior processability/flow and better chemical resistance when exposed to many automotive fluids over PX0844. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | dry; ISO 527 |
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
Eastman Tritan MX811 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO.. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | |
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe) Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | 2 in/min; ASTM Test |
BASF Ultraform N 2640 Z4 UNC Q600 POM Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | Wet; ASTM D638 |
Asahi Kasei Leona® 9400S Nylon 66 Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RKT 736 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific) LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO R527 |
Fainplast Compounds RI 52/C Rigid PVC, Injection Molding Electric fittings |